MEMBRANE DOOR
Zander membrane doors are manufactured using flush doors that are over laid with imported rigid membrane film of different and colours. The membrane prevents the doors from contracting, expanding, cracking, or separating at the joints. It’s easy to install and low maintenance of these doors as they do not require any form of polishing, painting or varnishing. Moreover, its availability in multiple colour shades, styles, designs and texture have enabled us to cater to any and every choice requirement of our clients.
Technical Data and General Specification of Zander Club Marine (BWP) Membrane Flush Door
TESTS | IS 2202 (Part 1) Requirements | OBSERVE VALUE |
---|---|---|
Workmanship and Finish | Satisfactory | Satisfactory |
Dimension and Squareness Test | Length & Width within a limit 5mm(+/-) Thickness within limit of 1 mm (+/-) Squareness ≤ 1 mm | Length = +5/-0 mm Width = +5/-0 mm Thickness = +/- 0.5-0.7 mm Within limit |
General Flatness | Twist, Warping & Cupping ≤ 6 mm | Within limit |
Local Planness | The depth of deviation ≤ 0.5 mm | Within limit |
Impact Indentation Test | Depth of indentation ≤ 0.2 mm | 0.1 mm |
Flexure Test | Any residual deflection ≤ 1/10 x Maximum deflection. Deflection at the maximum load ≤ 1/30 x length or ≤ 1/15 of width. | Within limit Within limit |
Edge loading Test | The deflection of the edge Load ≤ 5 mm ( At the maximum load ) Residual deflection of edge ≤ 0.5 mm ( After removal of the load ) Lateral buckling ≤ 2 mm | Approx 4 mm Within limit Approx 1.5 mm |
Shock Resistance Test | No visible damage in any part of the door after 25 blows on each end. | No visible damage & Delamination |
Buckling Test | No Detoriation allow. Residual deformation ≤ 5 mm Initial deflection ≤ 50 mm | Maximum 3.8 mm Maximum 40 mm |
Slamming Test | No visible damage in any part | No Damage |
Misuse Test | No permanent deformation | No deformation |
End immersion Test | No de-lamination after 8 cycles. Glue adhesion minimum pass standard after 8 cycles. | No de-lamination |
Knife Test | Minimum pass standard | Excellent |
Glue adhesion Test after Boiling. | No de-lamination allows. | No de-lamination |
Screw withdrawal Test | Required load ≤ 1000 N to withdraw the screw. No visible damage to the surface. | 2000 N No visible damage on surface |
Surface Resistance To Steam | After 1 hour No surface cracks, discolour and delamination Allowed | No any cause found |
Resistance To Cracking under Heat | After 24 Hour at 70 ±20C No surface cracks and delamination Allowed | No cracks and delamination found |
Resistance to Stain | No Blistering, staining or discoloration After 1500 Strokes | No any cause found |
Surface Membrane | High Quality PVC Membrane Foil about 0.25 - 1 mm thickness used | |
Core Composed | 100 % Composed core No Gaps or Overlaps with Smooth Surface | |
Species | Hardwood | 100 % Hardwood Species |
Filler | Hardwood | 100 % Hardwood Species use for Filler Which give a good strength to door |
Grade | Boiling Water Proof | Boiling Water Proof |
Resin Type | BWP Grade resin | BWP Grade PF Conventional Resin Used |
Virashield | Anti Viral, Anti Bacterial | To Reduce Viral And Bacterial Activity |
Chemically Treated | CCB Chemical | Borer & Fungus Proof Anti-Termite Resistance |