BLOCK BOARD

These are made out of excellent quality of plantation timbers. Logs are quarter sawn into planks using SDR method, which are chemically treated and well seasoned before converting into battens in a multiple ripsaw. Battens are sandwiched between glued mechanically dried veneers and are pressed in hot press under accurate temperature and pressure. Quarter, sawing of logs and proper seasoning of planks make it dimensionally stable and treatment of planks, poisoning of glue line and preservative treatment of finished block make Zander durable and safe against borers.
Block Board

Technical Specification Marine BWP Block Board

TestsAs Per Observe Value
Moisture Content 5-15%Within the range
Adhesion of piles
Water Resistance Test
(72hours boiling)
Minimum Pass Standard
No separation allowed
Minimum pass standard
Excellent
No separation found at any veneer line
Static bending strength
(N/MM2)
(MOR) along the grain-50Less than 50
Screw holding strength (KG)More than 150
Nail holding Strenghth (KG)More than 75
Water Absorption (%)More than 5
Core Composed100% composed core no gaps or overlaps with smooth surface
Species Hardwood 100% hardcore species
Filler PineHardwood used for filler which give more strength and durability in board
Resin TypeBWP grade resinConventional resin used
Virashield Anti viral, Anti bacterialTo reduce viral and bacterial activtiy
Chemically Treated CCB chemicalBorer & Fungus proof Anti-termite resistance
Resistance to MicroorganismsNo applicable sign of separation at edges.No separation at edges
Spot testEntire penetration of preservative chemicals through battenSatisfactory

OUR OTHER PRODUCTS